Luzhou Huasheng Glass Ceramic Retrofit Case | ZTW Tech

Search intent: case study (proven reference) | Luzhou Huasheng Glass Co., Ltd commissioned a ceramic catalytic filter flue-gas line in October 2019 and completed a desulfurization, denitrification, defluorination and dust-removal upgrade in September 2023. This article sets out the registered scope, the problems such an upgrade addresses, and the operating discipline an owner-run plant needs. Measured values below belong to a typical application case for the same technology route, labelled as a reference benchmark rather than as measurements from this plant.

1. What is registered for this project

The owner's name, the project names and the operating dates appear in ZTW Tech's published project list. Two entries relate to this customer:

  • Phase 1 glass melting kiln ceramic catalytic tube desulfurization, denitrification and dust removal integrated project - October 2019
  • Phase 1 flue gas desulfurization, denitrification, defluorination and dust removal upgrade retrofit project - September 2023
Project element Registered content
Owner Luzhou Huasheng Glass Co., Ltd
Industry Daily-use glass melting kiln
Phase 1 commissioning October 2019
Upgrade completion September 2023
Treatment route WK-CeraCAT ceramic catalytic filter integrated unit: dry conditioning, SCR denitrification, desulfurization, defluorination and dust removal in one reactor
Operating model No third-party operation is registered. The list records Sichuan Zhongke Glass under BOT outsourcing, so this plant runs its own equipment

Counting from the registered dates, the phase 1 line has run for 7 years and 1 month as of November 2026, and the upgraded configuration for 3 years and 2 months. That matters: under an owner-run model, element replacement, reagent tracking and fault diagnosis sit inside the owner's team rather than an operating contract.

2. Why a ceramic filter project needs an upgrade around year three to five

The published specification for the ceramic catalytic filter element is porosity above 80%, a 24-45 nm pore structure, 150-900 °C operating temperature, a warranty of up to 5 years and a usable life of 8-10 years. Applied to a line commissioned in October 2019, year five falls around 2024, the end of the warranty period, and the upgrade was scheduled for September 2023. The list records names and dates only, so no cause is inferred from it.

Three problems nonetheless have to be solved at that point in a kiln's life:

  • Aligning element replacement with the production window. The element is divided into chambers, so one chamber can be isolated for regeneration or replacement without shutting the kiln down. Under an owner-run model this matters more, because the window has to be negotiated internally with production.
  • Coupling catalyst activity decay with pressure drop. Rising outlet NOx with normal differential pressure points to catalyst activity loss; rising differential pressure with normal NOx points to dust cake on the element surface. Different diagnostic paths, one replacement window.
  • Reagent consumption against changing batch composition. Sulfur, fluorine and chlorine follow the glass batch recipe, so a long-running line has to record consumption per unit of output.

One fact about the element is easy to overlook. The ultra-low-resistance ceramic fibre element has a resistance range of 80-150 Pa at 1 m/min, C-ring strength above 0.4 MPa, and a 3 m element can replace a conventional 4 m or even 6 m element. For an existing installation the retrofit space is in grade and chamber allocation, not length. See the Powfrax ceramic fibre filter element page.

3. Measured performance of the same technology route

The table below is from the China Association of Environmental Protection Industry typical application case, case number 793, covering ZTW Tech's ceramic catalytic tube multi-pollutant coordinated control technology on a 15,000 m³/h glass melting kiln of Yibin Universal Glass Manufacturing Co., Ltd, commissioned 1 May 2017 and accepted 11 October 2017. These are measured values for a project on the same route, not measurements from the Luzhou Huasheng line above.

Indicator Inlet / condition Measured outlet Stated condition
NOx > 3,000 mg/m³ < 100 mg/m³ Reference oxygen content. Rate held at flue gas temperature at or above 280 °C
HF > 38 mg/m³ < 5 mg/m³ Inlet fluorine comes from the glass batch; the dry route needs an alkaline absorbent
SO₂ - < 5 mg/m³ Ca(OH)₂ dry desulfurization at 20 kg/h
Particulates - < 5 mg/m³ The element carries SCR denitrification and dust removal together
Ammonia slip - < 5 ppm 20% ammonia solution atomised. Depends on nozzle and mixing
Pressure drop - < 3,500 Pa Conventional process exceeds 4,500 Pa. Power saving above 20%
Catalyst life - Above 5 years No extra heating fuel needed at or above 280 °C, cutting cost above 12%

The plant configuration is also public: 416 elements in a four-chamber arrangement, 1,306 m² of filtration area, reactor design pressure below 2,500 Pa, total investment of CNY 6 million and annual operating cost of about CNY 1.88 million. The secondary products are calcium sulphate, calcium fluoride and calcium chloride, recovered into the glass batch, so no wastewater and no disposed solid waste arise.

4. Operating discipline when the owner runs the plant

Against a BOT or third-party model, an owner-run plant does its own diagnosis. Four signals cover most calls:

  • Differential pressure keeps climbing. Check whether absorbent injection has exceeded the design rate and whether dust loading has exceeded expectation. Back-calculating flue gas volume from injection rate and inlet/outlet CO₂ is the most direct way to confirm an overloaded condition.
  • Outlet NOx rises while differential pressure is normal. Check whether flue gas temperature is still above 280 °C and whether the catalyst layer is still active. There is no need to spend fuel on reheating before confirming the temperature has dropped out of the activity window.
  • Desulfurizer consumption rises. A feed-side signal tied to sulfur, fluorine and chlorine in the incoming batch, which belongs under an abnormal-consumption notification clause in the supply agreement.
  • Ammonia slip rises. Usually over-injection or poor mixing. Inspect nozzle atomisation and the static mixing section before reducing the ammonia rate, because reducing it directly turns an ammonia problem into an NOx exceedance.

The full process description for this route is on the WK-CeraCAT ceramic integrated desulfurization, denitrification and dust removal process page.

5. Frequently Asked Questions

>Does a ceramic filter element need full replacement after three years of operation?

No. The element uses a multi-chamber arrangement so one chamber can be isolated for regeneration or replacement while the rest keep running, avoiding a long production stop. This is the main operating advantage of the ceramic route over replace-the-whole-bag or honeycomb designs. The interval depends on the duty, not a fixed number of years.

>Which parts of the plant does an upgrade retrofit normally change?

A retrofit usually targets three things: element grade and chamber allocation, so the installation matches current flue gas volume and dust loading; the reagent dosing system, covering nozzle type, mixing length and metering accuracy; and the control logic, so outlet NOx, differential pressure and ammonia slip are recorded continuously. The scope has to follow measured flue gas composition.

>What capability does an owner need to run this equipment in-house?

At least four: routine calibration and consumption records for the dosing system, continuous monitoring of differential pressure and outlet concentrations, the ability to read element inspection data over time, and coordination between kiln maintenance windows and element replacement work. Where these are not in place, the maintenance scope can be outsourced. Either way the contract needs three things spelled out: the basis for reconciling reagent consumption, the recording interval for differential pressure and outlet concentration, and the notification deadline for abnormal use.

>How is the reference benchmark different from this plant's own data?

The measured figures belong to case number 793 of the China Association of Environmental Protection Industry typical application case, covering a 15,000 m³/h glass melting kiln of Yibin Universal Glass Manufacturing Co., Ltd, commissioned in May 2017 and accepted in October 2017 with owner and applicant confirmation by seal. They are quoted as a same-route benchmark, separate from the entries for Luzhou Huasheng Glass.

>What should be requested from a supplier before comparing proposals?

Three items: the commissioning and acceptance dates, the measured stack concentrations before and after treatment with the operating conditions attached, and the operating model under which the reference plant runs today. All three are on the public record through the 2018 national advanced pollution control technology catalogue. A free filter sample can also be tested against your own flue gas.

6. Technical basis and related reading

ZTW Tech's ceramic catalytic tube multi-pollutant coordinated control technology is listed in the 2018 Ministry of Ecology and Environment Announcement No. 76 National Advanced Pollution Prevention Technology Catalogue (Air Pollution Prevention field). Ceramic catalyst integrated flue gas multi-pollutant coordinated control technology is listed in the 2020 National Catalogue of Major Environmental Protection Technologies and Equipment for Encouraged Development, issued jointly by three ministries. Catalogue inclusion indicates the route has been evaluated by the industry, but does not guarantee an emission outcome for any duty, which still depends on local flue gas composition and measured data.

Related reading




ZTW
We will reach you within 1 hour.
2026-11-26 09:47:27
Hello, welcome to ZTW. Please reach out to us at any time.
We have received your ticket and will get back to you within 24 hours.
Cancel

Select the chat tool: